Sheet


material Mo
thickness
(inch)
0.0157
tol
(inch)
± 0.0008
width
(inch)
23.622
tol
(inch)
± 0.063
length
(inch)
78.740
tol
(inch)
+ 0.1969/- 0.0000
quality/
finish
bright
weight
(lb/pce)
10.803
More product informations bright, cold rolled, deep drawable
specification Download
 

article  12006534

Mo sheet .016" x 23.622" x 78.740"
bright


list price [USD]

<2,00 pce 
1.354,42/pce

≥2,00 pce 
1.128,69/pce

≥4,00 pce 
902,95/pce


 