Sheets


material Mo
thickness
(mm)
0,600
tol
(mm)
±0,028
width
(mm)
200,0
tol
(mm)
±1,600
length
(mm)
600,0
tol
(mm)
+5/-0
quality/
finish
ground
weight
(kg/pce)
0,734
More product informations ground, cold rolled, deep drawable
specification Download
 

article  257484

Mo sheet 0,6 x 200 x 600
ground


list price [EUR]

<5,00 pce 
202,09/pce

≥5,00 pce 
151,57/pce

≥12,00 pce 
126,31/pce

≥30,00 pce 
101,05/pce


 

Service number

Do you have any questions or require any further information?