SPARKAL® X rods


SPARKAL®X rod Dia 10 X 350 MM
material SPX
dia
(mm)
10,000
tol
(mm)
0/+0,22
length
(mm)
350,0
tol
(mm)
0/+1
weight
(kg/pce)
0,419