TIG Electrode


material WC20
dia
(mm)
3,200
length
(mm)
150,0
quality/
finish
colour: grey
More product informations annealed
specification Download
 

article  257576

WC20 TIG electrode Ø 3,2 x 150 mm
colour: grey


list price [EUR]

<160,00 pce 
5,63/pce

≥160,00 pce 
4,23/pce

≥400,00 pce 
3,52/pce

≥930,00 pce 
2,82/pce


 