Wire


material ML
dia
(mm)
0,800
tol
(mm)
±0,012
quality/
finish
electropolished
weight
(kg/1.000 m)
5,124
More product informations annealed, shipment on spool SD 300 K
specification Download
 

article  332235

ML wire Ø 0,80 mm (SD300K)
electropolished


list price [EUR]

<909,55 m 
1.099,45/1000 m

≥909,55 m 
824,59/1000 m

≥2.182,91 m 
687,16/1000 m

≥5.457,27 m 
549,73/1000 m


 