Evaporation coil wire

Evaporation coils made from tungsten, molybdenum, and tantalum

Thermal evaporation (resistance evaporation) is a coating method and is one of the PVD (Physical Vapor Deposition) processes. The material for the final layer is heated inside a vacuum chamber until it evaporates. The vapor of the material condensates on the substrate for the desired layer.

As resistance heaters, our evaporation coils have a very high melting point. This means that they can heat virtually any material to the highest temperatures.

Your advantages at a glance:

  • High corrosion
    resistance

  • Highly pure material prevents impurities on the substrate

  • High dimensional stability

The perfect material for your application

Our range includes evaporation coils made of the following materials:

  • WVM (grain-stabilized tungsten for vacuum metallizing) for evaporating aluminum
  • Tantalum
  • Molybdenum
  • Molybdenum-lanthanum (ML) for a particularly long service life

Standard dimensions at a glance

We have the following standard dimensions available in stock. We'll be happy to produce further dimensions according to your specific requirements. Simply get in touch.

Item
number
Coil designation Diameter
[mm]
Number of
strands
Length L
[mm]
Diameter
FD
[mm]
Coil
length FL
[mm]
Coil
spacing
P [mm]
11793590 SS05S3-100 0.5 3
100      
11793591 SS08S3-100 0.8 3
100      
11793597 SU05S3-100-1554P01 0.5 3
100 14.5 54 1.0
11793594 SU08S3-100-1554P01 0.8 3
100 14.5 54 1.0
11793599 SV08S3-100-1513P01 0.8 3
100 15.2 13 1.0
11793600 SV10S3-100-1914P01 1.0 3
100 19.5 14 1.0
11793601 SV05S3-100-1513P01 0.5 3
100 15.2 13 1.0
11738657 SH08S3-100-0644P04 0.8 3
100 6.4 44 4.0
11738666 SH08S3-100-0548P05 0.8 3
100 4.8 47.7 5.3
11738671 SH08S3-100-0648P08 0.8 3
100 6.4 48 8.0
11780142 SH05S3-100-0550P06 0.5 3
100 5.0 50 5.5
11740567 SH10S3-100-0750P08 1.0 3 100 6.5 50 8.3
11502785 SH10S3-100-0744P04 1.0 3 100 6.5 44 4.0
11738674 SB06S3-100-1114P02 0.6 3 100 10.5 14 2.1
11738679 SB10S1-080-1110P02 1.0 1 80
11.3 10 1.8
11780144 SB10S1-100-1110P02 1.0 1 100 11.3 10 1.8
11793603 SB05S3-100-1114P02 0.5 3 100 10.6 13.5 1.8
11793605 SB08S3-100-2329P04 0.8 3 100 23.1 29 3.67
11793606 SB08S3-100-1623P03 0.8 3 100 16.2 23.3 3.07
11793608 SB06S3-130-1114P02 0.6 3 130 10.5 14 2.1
11793609 SB08S3-100-1114P02 0.8 3 100 10.6 13.5 1.7
11793611 SB08S1-100-1114P02 0.8 1 100 10.6 13.5 1.8

Item numbers for evaporation coils

More detailed information regarding our evaporation coils can be derived from the item number. This is formulated as follows:

Item numbers for evaporation coils

    

Evaporation coil dimensions