Material
dia (mm)
0,400
0,500
0,600
0,635
0,700
0,760
0,800
1,000
2,000
2,500
3,000
quality/finish
electropolished
pickled
Number of products:13
Product list (.XLS)
ML wire Ø 0,40 mm (SH253K) electropolished
article: 332249
204,84 € - 409,68 € (1000 m )
(m)
Mo wire Ø 0,50 mm (SH253K) electropolished
article: 15903
296,24 € - 592,48 € (1000 m )
(m)
ML wire Ø 0.50 mm(SD300K) electropolished
article: 332240
308,16 € - 616,31 € (1000 m )
(m)
ML wire Ø 0,60 mm (SD300K) electropolished
article: 327698
435,15 € - 870,30 € (1000 m )
(m)
WVM wire Ø 0,635 mm (SH253K) pickled
article: 256123
1.814,50 € - 2.903,30 € (1000 m )
(m)
ML wire Ø 0,70 mm (SD300K) electropolished
article: 331052
580,65 € - 1.161,29 € (1000 m )
(m)
WVM wire Ø 0,760 mm (SH253K) pickled
article: 128489
2.333,20 € - 3.733,10 € (1000 m )
(m)
ML wire Ø 0,80 mm (SD300K) electropolished
article: 332235
743,11 € - 1.486,21 € (1000 m )
(m)
WVM wire Ø 1,00 mm (SD300K) pickled
article: 9157
4.738,20 € - 7.581,20 € (1000 m )
(m)
Mo wire Ø 1,00 mm (SH253K) electropolished
article: 150532
1.087,33 € - 2.174,67 € (1000 m )
(m)
Mo wire Ø 2,00 mm (Coil) pickled
article: 137259
3.857,48 € - 5.786,22 € (1000 m )
(m)
Mo wire Ø 2,50 mm (Coil) pickled
article: 128644
5.732,41 € - 8.598,62 € (1000 m )
(m)
Mo wire Ø 3,00 mm (Coil) pickled
article: 149948
8.254,67 € - 12.382,01 € (1000 m )
(m)
×
Please log in to our shop to be able to order. If you have no access, please complete the registration form.
LogIn
Registration form
Standard Products
Sheets
Rods
SPARKAL® EDM electrodes
Densimet® WR-filler metal
Ribbon
Wire
Evaporation boats
Furnace and standard parts
PVD-Targets